Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Wasserabsorption | 9.5 % Show Supplier Material materials with Wasserabsorption of 9.5 % | dry | Sim. to ISO 62 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 9e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-07 1/K | dry | ISO 11359-1/-2 | Parallel |
1e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1e-06 1/K | dry | ISO 11359-1/-2 | Normal | |
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Viscosity number | 160 cm³/gr Show Supplier Material materials with Viscosity number of 160 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |