Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.33 g/cm³ Show Supplier Material materials with Dichte of 1.33 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 0.2 % Show Supplier Material materials with Wasserabsorption of 0.2 % | dry | ISO 62 | at 23°C after 24h |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 300 % Show Supplier Material materials with Dehnung of 300 % | dry | ISO 527-1/-2 | ||
460 % Show Supplier Material materials with Dehnung of 460 % | dry | ISO 527-1/-2 | |||
530 % Show Supplier Material materials with Dehnung of 530 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | 0.33 GPa Show Supplier Material materials with Elastizitätsmodul of 0.33 GPa | dry | ISO 527-1/-2 | ||
Härte, Shore A | 98 [-] Show Supplier Material materials with Härte, Shore A of 98 [-] | dry | ISO 868 | 3s | |
98 [-] Show Supplier Material materials with Härte, Shore A of 98 [-] | dry | ISO 868 | 15s | ||
Härte, Shore D | 61 [-] Show Supplier Material materials with Härte, Shore D of 61 [-] | dry | ISO 868 | 15s | |
64 [-] Show Supplier Material materials with Härte, Shore D of 64 [-] | dry | ISO 868 | 3s | ||
Reißfestigkeit | 171 kN/m Show Supplier Material materials with Reißfestigkeit of 171 kN/m | dry | ISO 34-1; Method B | ||
187 kN/m Show Supplier Material materials with Reißfestigkeit of 187 kN/m | dry | ISO 34-1; Method B | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 3.7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3.7 kJ/m² | dry | ISO 179/1eA | |
23 °C | 23 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 23 kJ/m² | dry | ISO 179/1eA | ||
Zugfestigkeit | 34 MPa Show Supplier Material materials with Zugfestigkeit of 34 MPa | dry | ISO 527-1/-2 | Normal | |
36 MPa Show Supplier Material materials with Zugfestigkeit of 36 MPa | dry | ISO 527-1/-2 |
Thermisch
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.3 [-] | dry | IEC 62631-2-1 | 100Hz |
Durchschlagfestigkeit | 14.4 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 14.4 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 | |
Verlustfaktor | 495 [-] Show Supplier Material materials with Verlustfaktor of 495 [-] | dry | IEC 62631-2-1 | 1MHz |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 15 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 15 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire and Cable Insulation | |
Certifications | Yellow Card Available |