Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.36 g/cm³ Show Supplier Material materials with Dichte of 1.36 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 2.2 % Show Supplier Material materials with Wasserabsorption of 2.2 % | dry | ISO 62 | at 23°C after 24h |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Biegemodul | 5 GPa Show Supplier Material materials with Biegemodul of 5 GPa | conditioned | ISO 178 | |||
7.5 GPa Show Supplier Material materials with Biegemodul of 7.5 GPa | dry | ISO 178 | ||||
Dehnung | 2.9 % Show Supplier Material materials with Dehnung of 2.9 % | dry | ISO 527-1/-2 | 1 mm | ||
3.2 % Show Supplier Material materials with Dehnung of 3.2 % | dry | ISO 527-1/-2 | 1 mm | |||
3.4 % Show Supplier Material materials with Dehnung of 3.4 % | conditioned | ISO 527-1/-2 | ||||
Elastizitätsmodul | 5 GPa Show Supplier Material materials with Elastizitätsmodul of 5 GPa | conditioned | ISO 527-1/-2 | |||
7.5 GPa Show Supplier Material materials with Elastizitätsmodul of 7.5 GPa | dry | ISO 527-1/-2 | 1 mm | |||
7.5 GPa Show Supplier Material materials with Elastizitätsmodul of 7.5 GPa | dry | ISO 527-1/-2 | 1 mm | |||
Flexural yield strength | 140 MPa Show Supplier Material materials with Flexural yield strength of 140 MPa | conditioned | ISO 178 | |||
190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | dry | ISO 178 | ||||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | conditioned | ISO 179/1eA | |||
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 49 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 49 kJ/m² | dry | ISO 179/1eU | ||
23 °C | 53 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 53 kJ/m² | conditioned | ISO 179/1eU | |||
Zugfestigkeit | 85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | conditioned | ISO 527-1/-2 | |||
120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | dry | ISO 527-1/-2 | 1 mm | |||
130 MPa Show Supplier Material materials with Zugfestigkeit of 130 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Koeffizient der thermischen Ausdehnung | 2.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 120 °C Show Supplier Material materials with Relative temperature index, electrical of 120 °C | dry | UL746B | 0.2 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.2 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.2 mm | ||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 285 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 285 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.6 [-] | dry | IEC 60250 | 1GHz |
3.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.6 [-] | dry | IEC 60250 | 10GHz | |
3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | conditioned | IEC 60250 | 10GHz | |
3.75 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.75 [-] | conditioned | IEC 60250 | 1GHz | |
Durchschlagfestigkeit | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | conditioned | IEC 60243-1 | |
33 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 33 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 550 V Show Supplier Material materials with Kriechstromfestigkeit of 550 V | dry | IEC 60112 | |
Surface resistivity | 7e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 7e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 100 [-] Show Supplier Material materials with Verlustfaktor of 100 [-] | dry | IEC 60250 | 1GHz |
100 [-] Show Supplier Material materials with Verlustfaktor of 100 [-] | dry | IEC 60250 | 10GHz | |
180 [-] Show Supplier Material materials with Verlustfaktor of 180 [-] | conditioned | IEC 60250 | 10GHz | |
210 [-] Show Supplier Material materials with Verlustfaktor of 210 [-] | conditioned | IEC 60250 | 1GHz | |
Volume resistivity | 4e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 4e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Reflow connectors (2) | |
Certifications | Yellow Card Available | |
Fillers | 20% Glass Fiber |