Property | Value | Comment |
---|---|---|
Dichte | 1.05 g/cm³ Show Supplier Material materials with Dichte of 1.05 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 67.35 MPa Show Supplier Material materials with Biegefestigkeit of 67.35 MPa | ASTM D790 |
Biegemodul | 2.35 GPa Show Supplier Material materials with Biegemodul of 2.35 GPa | ASTM D790 |
Dehnung | 30.0 % Show Supplier Material materials with Dehnung of 30.0 % | ASTM D638 |
Elastizitätsmodul | 2.15 GPa Show Supplier Material materials with Elastizitätsmodul of 2.15 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 250.0 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 250.0 J/m | ASTM D256 |
Zugfestigkeit | 42.5 MPa Show Supplier Material materials with Zugfestigkeit of 42.5 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Schmelzpunkt | 180.0 - 200.0 °C Show Supplier Material materials with Schmelzpunkt of 180.0 - 200.0 °C | ISO 3146-C | |
Vicat-Erweichungstemperatur | 94 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 94 °C | ASTM D1525 | |
Entflammbarkeit | UL-94 1/16‘ HB |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 44.0 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 44.0 g/10min | ASTM D1238 |
Schrumpfung | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | The strength, flexibility, machinability and high-temperature resistance of ABS often makes it the plastic preferred by engineers and people intending to use plastic in a mechanical context. | |
Certifications | Extrudr ABS can be used in applications for direct/indirect food contact under the FDA regulation | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |