Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Bio-based content | 90 % Show Supplier Material materials with Bio-based content of 90 % | ||
Dichte | 23.0 °C | 1.15 g/cm³ Show Supplier Material materials with Dichte of 1.15 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 7.12 GPa Show Supplier Material materials with Biegemodul of 7.12 GPa | ISO 527 |
Dehnung | 23.0 °C | 2.8 % Show Supplier Material materials with Dehnung of 2.8 % | ISO 527 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 4.6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.6 kJ/m² | ISO 179-1/1 eA |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 82 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 82 kJ/m² | ISO 179-1/1 eU |
Zugfestigkeit | 23.0 °C | 65 MPa Show Supplier Material materials with Zugfestigkeit of 65 MPa | ISO 527 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 115 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 115 °C | ISO 75/B |
Schmelzpunkt | 190 - 240 °C Show Supplier Material materials with Schmelzpunkt of 190 - 240 °C | ISO 3146-C |
Vicat-Erweichungstemperatur | 165 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 165 °C | ISO 306 |
Wärmeformbeständigkeitstemperatur | 115 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 115 °C |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | GreenTEC PRO Carbon is designed for extreme industrial use. It has very good mechanical and thermal properties | |
Fillers | 10% Carbon Fiber | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |