Property | Value | Comment |
---|---|---|
Dichte | 1.3 g/cm³ Show Supplier Material materials with Dichte of 1.3 g/cm³ | ASTM D792 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 68.3 MPa Show Supplier Material materials with Biegefestigkeit of 68.3 MPa | ISO 178 |
Biegemodul | 3.1 GPa Show Supplier Material materials with Biegemodul of 3.1 GPa | ISO 527 |
Dehnung | 29.0 % Show Supplier Material materials with Dehnung of 29.0 % | ISO 527 |
Elastizitätsmodul | 2.04 GPa Show Supplier Material materials with Elastizitätsmodul of 2.04 GPa | ISO 178 |
Zugfestigkeit | 50.0 MPa Show Supplier Material materials with Zugfestigkeit of 50.0 MPa | ISO 527 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 180.0 - 200.0 °C Show Supplier Material materials with Schmelzpunkt of 180.0 - 200.0 °C | ISO 3146-C |
Vicat-Erweichungstemperatur | 78 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 78 °C | ISO 306 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 7.0 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 7.0 g/10min | ISO 1133 |
Schrumpfung | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | ISO 294-4 |
Technological properties
Property | ||
---|---|---|
Application areas | PETG is specifically designed to have a large and general scope of application in situations where the main requirement is the balance between mechanical and optical material properties. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |