Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Bio-based content | 100 % Show Supplier Material materials with Bio-based content of 100 % | ||
Dichte | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Dichte of 1.45 g/cm³ | ISO 2781 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 30 MPa Show Supplier Material materials with Biegefestigkeit of 30 MPa | ISO 527 |
Biegemodul | 23.0 °C | 3.4 GPa Show Supplier Material materials with Biegemodul of 3.4 GPa | ISO 527 |
Dehnung | 23.0 °C | 22.3 % Show Supplier Material materials with Dehnung of 22.3 % | ISO 527 |
Zugfestigkeit | 23.0 °C | 43 MPa Show Supplier Material materials with Zugfestigkeit of 43 MPa | ISO 527 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 160 - 200 °C Show Supplier Material materials with Schmelzpunkt of 160 - 200 °C | |
Vicat-Erweichungstemperatur | 48 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 48 °C | ISO 306 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 15 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 15 g/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Flax enables a high printing speed and therefore saves time, which is why it is often used in rapid prototyping. | |
Chemical composition | Biodegradable batch based on PLA, contains copolyester and additives. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year |