Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 1.15 g/cm³ Show Supplier Material materials with Dichte of 1.15 g/cm³ | ISO 2781 |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Shore A | 98.0 [-] Show Supplier Material materials with Härte, Shore A of 98.0 [-] | ISO 868 |
Reißfestigkeit unverstärkt | 176.0 kN/m Show Supplier Material materials with Reißfestigkeit unverstärkt of 176.0 kN/m | ISO 34-1B |
Zugfestigkeit | 42.0 MPa Show Supplier Material materials with Zugfestigkeit of 42.0 MPa | ISO 527-2 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 180.0 - 200.0 °C Show Supplier Material materials with Schmelzpunkt of 180.0 - 200.0 °C | ISO 3146-C |
Vicat-Erweichungstemperatur | 110 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 110 °C | ISO 306 |
Technological properties
Property | ||
---|---|---|
Application areas | Due to its chemical and mechanical resistance, TPU is primarily used in the car and footwear industry. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |