Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 3.3 GPa Show Supplier Material materials with Biegemodul of 3.3 GPa | ISO 527 |
Dehnung | 23.0 °C | 14 % Show Supplier Material materials with Dehnung of 14 % | ISO 527 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 19 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 19 kJ/m² | ISO 179-1/1 eA |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 218 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 218 kJ/m² | ISO 179-1/1 eU |
Zugfestigkeit | 23.0 °C | 45 MPa Show Supplier Material materials with Zugfestigkeit of 45 MPa | ISO 527 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 47 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 47 °C | ISO 75/B |
Schmelzpunkt | 180 - 200 °C Show Supplier Material materials with Schmelzpunkt of 180 - 200 °C | ISO 3146-C |
Vicat-Erweichungstemperatur | 115 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 115 °C | ISO 306 |
Wärmeformbeständigkeitstemperatur | 47 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 47 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 3.5 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 3.5 g/10min | ISO 1133 | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | ISO 294-4 |
Technological properties
Property | ||
---|---|---|
Application areas | GreenTEC is designed for industrial use. It has good mechanical and thermal properties. | |
Handling recommendations | Store at room temperature (18-27°C / 65-80°F), out of direct heat and sunlight, and in a dry place. When stored correctly, this material has a shelf life of 1 year. |