Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.7 g/cm³ Show Supplier Material materials with Dichte of 7.7 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 55 - 65 % Show Supplier Material materials with Dehnung of 55 - 65 % |
Flächenreduzierung | 23.0 °C | 65 - 75 % Show Supplier Material materials with Flächenreduzierung of 65 - 75 % |
Streckgrenze Rp 0,2 | 23.0 °C | 610 - 720 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 610 - 720 MPa |
Zugfestigkeit | 23.0 °C | 980 - 1120 MPa Show Supplier Material materials with Zugfestigkeit of 980 - 1120 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 16 - 20 % Show Supplier Material materials with Chrom of 16 - 20 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.15 % Show Supplier Material materials with Kohlenstoff of 0.15 % | max. | |
Mangan | 12 - 16 % Show Supplier Material materials with Mangan of 12 - 16 % | ||
Molybdän | 2.5 - 4.2 % Show Supplier Material materials with Molybdän of 2.5 - 4.2 % | ||
Niobium | 0.25 % Show Supplier Material materials with Niobium of 0.25 % | max. | |
Stickstoff | 0.75 - 1 % Show Supplier Material materials with Stickstoff of 0.75 - 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | The Ni-free steel grade P 2000 shows excellent biocompatibility and will be used mainly in contact with the human body, for the production of spectacle frames, watch cases and jewellery and after biological evaluation for the production of prosthesis for orthopaedics, bone screws and plates for osteosynthesis and high-strength wire for orthodontia. Additional applications result inevitably in cases where corrosion resistance, reliability and a high fa-tigue resistance are required. Examples are ultra high strength screws, nuts and bolts for the fastener industry. |