Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Ti 6Al-6V-2Sn
Titanium 6-6-2 is a heat treatable high strength titanium alloy with lower toughness and ductility than Titanium 6Al/4V. Titanium 6-6-2 has a similar machinability to Austenitic steel , easily welded providing precautions are taken to shield against Oxygen, Hydrogen and Nitrogen contaminants
Diese Materialdaten wurden von Hempel Special Metals zur Verfügung gestellt
All categories
Technological properties
Property | ||
---|---|---|
Application areas | Ordinance components Airframe Rocket case applications Pressure canisters |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.