Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7 g/cm³ Show Supplier Material materials with Dichte of 7 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Härte, Brinell | 23.0 °C | 270 [-] Show Supplier Material materials with Härte, Brinell of 270 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 21 - 23 % Show Supplier Material materials with Chrom of 21 - 23 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | max. | |
Kupfer | 0.11 % Show Supplier Material materials with Kupfer of 0.11 % | max. | |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % | max. | |
Nickel | 2.5 - 3.5 % Show Supplier Material materials with Nickel of 2.5 - 3.5 % | ||
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % | max. | |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | max. | |
Stickstoff | 0.1 - 0.22 % Show Supplier Material materials with Stickstoff of 0.1 - 0.22 % |
Technological properties
Property | ||
---|---|---|
Application areas | 1.4462 is used mainly in sector of chemical industry, petrochemical industry, offshore, sea water lines, sea water desalination plants, nuclear engineering, paper and pulp industry. |