Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 4.51 g/cm³ Show Supplier Material materials with Dichte of 4.51 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 18 % Show Supplier Material materials with Dehnung A50 of 18 % | min. |
Elastizitätsmodul | 23.0 °C | 105 GPa Show Supplier Material materials with Elastizitätsmodul of 105 GPa | |
Härte, Brinell | 23.0 °C | 170 [-] Show Supplier Material materials with Härte, Brinell of 170 [-] | max. |
Streckgrenze Rp 0,2 | 23.0 °C | 345 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 345 MPa | min. |
Zugfestigkeit | 23.0 °C | 480 MPa Show Supplier Material materials with Zugfestigkeit of 480 MPa | min |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 5.2E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.2E-7 Ω·m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Andere | 0.4 % Show Supplier Material materials with Andere of 0.4 % | total | |
Eisen | 0.03 % Show Supplier Material materials with Eisen of 0.03 % | max. | |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. | |
Mangan | 0.2 - 0.4 % Show Supplier Material materials with Mangan of 0.2 - 0.4 % | ||
Nickel | 0.6 - 0.9 % Show Supplier Material materials with Nickel of 0.6 - 0.9 % | ||
Sauerstoff | 0.25 % Show Supplier Material materials with Sauerstoff of 0.25 % | max. | |
Stickstoff | 0.03 % Show Supplier Material materials with Stickstoff of 0.03 % | max. | |
Titan | Balance | ||
Wasserstoff | 0.02 % Show Supplier Material materials with Wasserstoff of 0.02 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Ti Gr 12 semi-finished products are used in some areas, but the material is mainly used in the chemical industry and in the manufacture of pressure vessels. | |
Corrosion properties | Titanium Gr.12 offers excellent corrosion resistance to acids as well as very good resistance to crevice corrosion in hot brines. Due to the higher strength, Titanium Gr.12 can be used with a thinner wall thickness than Titanium Gr.2 or Titanium Gr.7 under the same conditions. | |
Other | We are pleased to offer you powder for 3D printing made of Titan Grade 12 / 3.7105 / UNS N53400 |