Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.81 g/cm³ Show Supplier Material materials with Dichte of 7.81 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -40.0 °C | 35 J Show Supplier Material materials with Charpy impact energy, V-notch of 35 J | min. |
23.0 °C | 80 J Show Supplier Material materials with Charpy impact energy, V-notch of 80 J | min. | |
Dehnung | 23.0 °C | 25 % Show Supplier Material materials with Dehnung of 25 % | min. |
Elastizitätsmodul | 23.0 °C | 199 GPa Show Supplier Material materials with Elastizitätsmodul of 199 GPa | |
Flächenreduzierung | 23.0 °C | 45 % Show Supplier Material materials with Flächenreduzierung of 45 % | min. |
Härte, Brinell | 23.0 °C | 270 [-] Show Supplier Material materials with Härte, Brinell of 270 [-] | max. |
Streckgrenze Rp 0,2 | 23.0 °C | 550 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 550 MPa | min. |
Zugfestigkeit | 23.0 °C | 750 MPa Show Supplier Material materials with Zugfestigkeit of 750 MPa | min. |
Magnetisch
Property | Temperature | Value |
---|---|---|
Relative magnetische Permeabilität | 23.0 °C | 33 [-] Show Supplier Material materials with Relative magnetische Permeabilität of 33 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 24 - 26 % Show Supplier Material materials with Chrom of 24 - 26 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | max. | |
Kupfer | 0.5 - 1 % Show Supplier Material materials with Kupfer of 0.5 - 1 % | ||
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % | max. | |
Molybdän | 3 - 4 % Show Supplier Material materials with Molybdän of 3 - 4 % | ||
Nickel | 6 - 8 % Show Supplier Material materials with Nickel of 6 - 8 % | ||
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. | |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % | max. | |
Silizium | 0.01 % Show Supplier Material materials with Silizium of 0.01 % | max. | |
Stickstoff | 0.2 - 0.3 % Show Supplier Material materials with Stickstoff of 0.2 - 0.3 % | ||
Wolfram | 0.5 - 1 % Show Supplier Material materials with Wolfram of 0.5 - 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Providing higher strengths than both austenitic and 22% Cr Duplex Stainless Steels UNS S32760 (F55) is suited to a variety of applications in industries such as Oil & Gas, CPI(Chemical Processing Industries), and Marine environments. | |
Corrosion properties | Super Duplex S32760/ F55 , Super Duplex Alloy UNS S32760 (F55 / 1.4501) has excellent resistance Pitting and Crevice Corrosion in seawater at elevated temperatures, supplied with a PREN 40<( Pitting Resistance Eqv) . Excellent resistance to SCC ( Stress Corrosion Cracking) in Sour and Chloride environments | |
Other | The material comes with a 3.1 certification. 3.2 certification are available with surcharge. |