Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Dichte of 8.9 g/cm³ |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1435 - 1445 °C Show Supplier Material materials with Schmelzpunkt of 1435 - 1445 °C |
Chemical properties
Property | Value |
---|---|
Eisen | 0.04 % Show Supplier Material materials with Eisen of 0.04 % |
Kohlenstoff | 0.02 % Show Supplier Material materials with Kohlenstoff of 0.02 % |
Kupfer | 0.25 % Show Supplier Material materials with Kupfer of 0.25 % |
Magnesium | 0.15 % Show Supplier Material materials with Magnesium of 0.15 % |
Mangan | 0.35 % Show Supplier Material materials with Mangan of 0.35 % |
Nickel | 90 % Show Supplier Material materials with Nickel of 90 % |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % |
Silizium | 0.2 % Show Supplier Material materials with Silizium of 0.2 % |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 201 is commonly used in food industry, but it is also in used vessels up to 600°C and sodium hydroxide evaporators up to 450°C. Alloy 201 is also often used in vessels for production of flour, hydrochloric acid or vinylchloride monomer. | |
Welding | Filler metal (for welding with 2.4066/2.4068) |