Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.61 g/cm³ Show Supplier Material materials with Dichte of 8.61 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schlagfestigkeit, Charpy gekerbt | -96.0 °C | 1200 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 1200 kJ/m² | min. |
23.0 °C | 1500 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 1500 kJ/m² | min. | |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1355 - 1400 °C Show Supplier Material materials with Schmelzpunkt of 1355 - 1400 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 20 - 22.5 % Show Supplier Material materials with Chrom of 20 - 22.5 % | |
Eisen | 2 - 6 % Show Supplier Material materials with Eisen of 2 - 6 % | |
Kobalt | 2.5 % Show Supplier Material materials with Kobalt of 2.5 % | max. |
Kohlenstoff | 0.01 % Show Supplier Material materials with Kohlenstoff of 0.01 % | max. |
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % | max. |
Molybdän | 12.5 - 14.5 % Show Supplier Material materials with Molybdän of 12.5 - 14.5 % | |
Nickel | 50 - 63 % Show Supplier Material materials with Nickel of 50 - 63 % | |
Schwefel | 5E-3 % Show Supplier Material materials with Schwefel of 5E-3 % | max. |
Silizium | 0.08 % Show Supplier Material materials with Silizium of 0.08 % | max. |
Vanadium | 0.35 % Show Supplier Material materials with Vanadium of 0.35 % | max. |
Wolfram | 2.5 - 3.5 % Show Supplier Material materials with Wolfram of 2.5 - 3.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 22 is used in the petrochemical and chemical industry. 2.4602 is a common material when it comes to contact with hot, contaminated mineral acids, solutions or seawater. It is used also in bleaching containers (such as in the pulp and paper industry) and acetic acid production in a reactor. Alloy 22 also occurs in components with sour gas applications. | |
Corrosion properties | Alloy C22 is very resistant to many corrosive media under oxidizing and reducing conditions. It is, for example, resistant to: | |
Welding | Welding Rod (WIG) 2.4635 |