Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.4 g/cm³ Show Supplier Material materials with Dichte of 8.4 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 1500 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 1500 kJ/m² | max. |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1330 - 1380 °C Show Supplier Material materials with Schmelzpunkt of 1330 - 1380 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.6 - 1.5 % Show Supplier Material materials with Aluminium of 0.6 - 1.5 % | |
Bor | 6E-3 % Show Supplier Material materials with Bor of 6E-3 % | max. |
Chrom | 20 - 23 % Show Supplier Material materials with Chrom of 20 - 23 % | |
Eisen | 2 % Show Supplier Material materials with Eisen of 2 % | max. |
Kobalt | 10 - 13 % Show Supplier Material materials with Kobalt of 10 - 13 % | |
Kohlenstoff | 0.05 - 1 % Show Supplier Material materials with Kohlenstoff of 0.05 - 1 % | |
Kupfer | 0.5 % Show Supplier Material materials with Kupfer of 0.5 % | max. |
Mangan | 0.7 % Show Supplier Material materials with Mangan of 0.7 % | max. |
Molybdän | 8 - 10 % Show Supplier Material materials with Molybdän of 8 - 10 % | |
Phosphor | 0.01 % Show Supplier Material materials with Phosphor of 0.01 % | max. |
Schwefel | 8E-3 % Show Supplier Material materials with Schwefel of 8E-3 % | max. |
Silizium | 0.7 % Show Supplier Material materials with Silizium of 0.7 % | max. |
Titan | 0.02 - 0.5 % Show Supplier Material materials with Titan of 0.02 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 617 is applied at high temperatures. Alloy 617 is used in air heaters, furnace components, beam pipes or high-temperature heat exchangers as well as in gas turbines and combustion chambers. | |
Welding | Welding Rods: FM 617- 2.4627 Wire Electrodes: Covered Rod Electrodes: |