Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.44 g/cm³ Show Supplier Material materials with Dichte of 8.44 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 1250 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 1250 kJ/m² | min. |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1290 - 1350 °C Show Supplier Material materials with Schmelzpunkt of 1290 - 1350 °C |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.4 % Show Supplier Material materials with Aluminium of 0.4 % | ||
Chrom | 21 - 23 % Show Supplier Material materials with Chrom of 21 - 23 % | ||
Eisen | 0.4 % Show Supplier Material materials with Eisen of 0.4 % | max. | |
Kobalt | 1 % Show Supplier Material materials with Kobalt of 1 % | max. | |
Kohlenstoff | 0.03 % Show Supplier Material materials with Kohlenstoff of 0.03 % | ||
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % | max. | |
Molybdän | 8 - 10 % Show Supplier Material materials with Molybdän of 8 - 10 % | ||
Nickel | Balance | ||
Niobium | 3.2 - 3.8 % Show Supplier Material materials with Niobium of 3.2 - 3.8 % | Ta+Nb | |
Phosphor | 0.01 % Show Supplier Material materials with Phosphor of 0.01 % | max. | |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % | max. | |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | max. | |
Tantal | 3.2 - 3.8 % Show Supplier Material materials with Tantal of 3.2 - 3.8 % | Ta+Nb | |
Titan | 0.4 % Show Supplier Material materials with Titan of 0.4 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | 2.4856 is used for: | |
Corrosion properties | In annealed condition (grade 1) Alloy 625: | |
Other | Annealed Alloy 625 loses notched impact strength at room temperature after having been exposed to temperatures in the range from 538 ° C to 593 ° C | |
Welding | Welding rods and wire electrodes: Covered electrodes: |