Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.9 g/cm³ Show Supplier Material materials with Dichte of 7.9 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 690 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 690 kJ/m² |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 1.8 - 2.4 % Show Supplier Material materials with Aluminium of 1.8 - 2.4 % | ||
Chrom | 24 - 26 % Show Supplier Material materials with Chrom of 24 - 26 % | ||
Eisen | 8 - 11 % Show Supplier Material materials with Eisen of 8 - 11 % | ||
Kohlenstoff | 0.15 - 0.25 % Show Supplier Material materials with Kohlenstoff of 0.15 - 0.25 % | ||
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % | max. | |
Mangan | 0.5 % Show Supplier Material materials with Mangan of 0.5 % | max. | |
Nickel | Balance | ||
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. | |
Schwefel | 0.01 % Show Supplier Material materials with Schwefel of 0.01 % | max. | |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. | |
Titan | 0.1 - 0.2 % Show Supplier Material materials with Titan of 0.1 - 0.2 % | ||
Ytterbium | 0.05 - 0.12 % Show Supplier Material materials with Ytterbium of 0.05 - 0.12 % | ||
Zirkonium | 0.01 % Show Supplier Material materials with Zirkonium of 0.01 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy 602 is versatile. Typical applications of Alloy 602CA are, i.e.: | |
Welding | Alloy 602CA can be welded using 2.4649 and DIN EN ISO 18274: S Ni 6025 as filler metal Covered electrodes: |