Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 4.51 g/cm³ Show Supplier Material materials with Dichte of 4.51 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Supplier Material materials with Dehnung A50 of 15 % | min., Annealed, specification values (ASTM F67) |
Streckgrenze Rp 0,2 | 23.0 °C | 483 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 483 MPa | min., Annealed, specification values (ASTM F67) |
Zugfestigkeit | 23.0 °C | 550 MPa Show Supplier Material materials with Zugfestigkeit of 550 MPa | min., Annealed, specification values (ASTM F67) |
Chemical properties
Property | Value |
---|---|
Eisen | 0.3 % Show Supplier Material materials with Eisen of 0.3 % |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % |
Sauerstoff | 0.25 % Show Supplier Material materials with Sauerstoff of 0.25 % |
Stickstoff | 0.03 % Show Supplier Material materials with Stickstoff of 0.03 % |
Titan | Balance |
Wasserstoff | 0.02 % Show Supplier Material materials with Wasserstoff of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | Ti Gr.4 is used in the chemical industry, aviation and aerospace. Due to its very good biocompatibility, it is also used in medicine. |