Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 4.43 g/cm³ Show Supplier Material materials with Dichte of 4.43 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Supplier Material materials with Dehnung A50 of 15 % |
Hardness, Rockwell | 23.0 °C | 34 [-] Show Supplier Material materials with Hardness, Rockwell of 34 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 880 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 880 MPa |
Zugfestigkeit | 23.0 °C | 950 MPa Show Supplier Material materials with Zugfestigkeit of 950 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1650 °C Show Supplier Material materials with Schmelzpunkt of 1650 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 5.5 - 6.75 % Show Supplier Material materials with Aluminium of 5.5 - 6.75 % | |
Titan | 88.74 - 91 % Show Supplier Material materials with Titan of 88.74 - 91 % | |
Vanadium | 3.5 - 4.5 % Show Supplier Material materials with Vanadium of 3.5 - 4.5 % | |
Wasserstoff | 0.02 % Show Supplier Material materials with Wasserstoff of 0.02 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Titanium Grade 5 is found as most used alloy in many areas again. Thus, for example in: | |
Welding | As filler for titanium grade 5 titanium bare wire of the same group can be used. |