Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 4.43 g/cm³ Show Supplier Material materials with Dichte of 4.43 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 10 % Show Supplier Material materials with Dehnung A50 of 10 % | min. |
Streckgrenze Rp 0,2 | 23.0 °C | 780 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 780 MPa | |
Zugfestigkeit | 23.0 °C | 860 MPa Show Supplier Material materials with Zugfestigkeit of 860 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 5.5 - 6.5 % Show Supplier Material materials with Aluminium of 5.5 - 6.5 % | ||
Eisen | 0.25 % Show Supplier Material materials with Eisen of 0.25 % | max. | |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. | |
Stickstoff | 0.05 % Show Supplier Material materials with Stickstoff of 0.05 % | max. | |
Titan | Balance | ||
Vanadium | 3.5 - 4.5 % Show Supplier Material materials with Vanadium of 3.5 - 4.5 % | ||
Wasserstoff | 0.01 % Show Supplier Material materials with Wasserstoff of 0.01 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Titanium Grade 23 ELI is found as most used alloy in medical industry for shoulder implants, hip-balls osteosyntheses, bone screws, bone plates, marrow-nails, spinalsystems, dental implants and tools. It's used also for: |