Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 4.51 g/cm³ Show Supplier Material materials with Dichte of 4.51 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 830 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 830 kJ/m² |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1670 °C Show Supplier Material materials with Schmelzpunkt of 1670 °C |
Chemical properties
Property | Value |
---|---|
Blei | 0.12 - 0.2 % Show Supplier Material materials with Blei of 0.12 - 0.2 % |
Eisen | 0.25 % Show Supplier Material materials with Eisen of 0.25 % |
Kohlenstoff | 0.06 % Show Supplier Material materials with Kohlenstoff of 0.06 % |
Sauerstoff | 0.18 % Show Supplier Material materials with Sauerstoff of 0.18 % |
Stickstoff | 0.05 % Show Supplier Material materials with Stickstoff of 0.05 % |
Titan | 99.3 % Show Supplier Material materials with Titan of 99.3 % |
Wasserstoff | 0.01 % Show Supplier Material materials with Wasserstoff of 0.01 % |
Technological properties
Property | ||
---|---|---|
Application areas | Titanium Grade 7 is preferably used in chemical plants. | |
Welding | As filler material for titanium grade 7 bare wire of the same titanium group should be used |