Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Hardness, Rockwell | 23.0 °C | 50 - 60 [-] Show Supplier Material materials with Hardness, Rockwell of 50 - 60 [-] | After hardening |
Härte, Vickers | 23.0 °C | 650 - 700 [-] Show Supplier Material materials with Härte, Vickers of 650 - 700 [-] | After hardening |
Zugfestigkeit | 23.0 °C | 900 MPa Show Supplier Material materials with Zugfestigkeit of 900 MPa | max., annealed |
Chemical properties
Property | Value |
---|---|
Chrom | 14 - 16 % Show Supplier Material materials with Chrom of 14 - 16 % |
Eisen | Balance |
Kohlenstoff | 0.25 - 0.35 % Show Supplier Material materials with Kohlenstoff of 0.25 - 0.35 % |
Molybdän | 0.85 - 1.1 % Show Supplier Material materials with Molybdän of 0.85 - 1.1 % |
Stickstoff | 0.3 - 0.4 % Show Supplier Material materials with Stickstoff of 0.3 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Cutting tools, surgical instruments (drills, mills etc.) screwdriver. |