Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 16 % Show Supplier Material materials with Dehnung of 16 % | min. |
Zugfestigkeit | 23.0 °C | 750 - 897 MPa Show Supplier Material materials with Zugfestigkeit of 750 - 897 MPa | min.:ISO 5832-12 and max.: ASTM F1537 |
Chemical properties
Property | Value |
---|---|
Chrom | 26 - 30 % Show Supplier Material materials with Chrom of 26 - 30 % |
Eisen | 0.75 % Show Supplier Material materials with Eisen of 0.75 % |
Kobalt | Balance |
Kohlenstoff | 0.35 % Show Supplier Material materials with Kohlenstoff of 0.35 % |
Mangan | 1 % Show Supplier Material materials with Mangan of 1 % |
Molybdän | 5 - 7 % Show Supplier Material materials with Molybdän of 5 - 7 % |
Nickel | 1 % Show Supplier Material materials with Nickel of 1 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Stickstoff | 0.25 % Show Supplier Material materials with Stickstoff of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Joint replacement for hip knee, shoulder etc. marrow-nails and dental application. This material can also be used for watch cases as it has an outstanding polishing ability and corrosion resistance. |