Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.15 g/cm³ Show Supplier Material materials with Dichte of 8.15 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 40 % Show Supplier Material materials with Dehnung A50 of 40 % | min., Annealed, Descaled |
Härte, Brinell | 23.0 °C | 130 [-] Show Supplier Material materials with Härte, Brinell of 130 [-] | Annealed, Descaled |
Streckgrenze Rp 0,2 | 23.0 °C | 248 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 248 MPa | Annealed, Descaled |
Zugfestigkeit | 23.0 °C | 490 MPa Show Supplier Material materials with Zugfestigkeit of 490 MPa | Annealed, Descaled |
Chemical properties
Property | Value |
---|---|
Eisen | Balance |
Nickel | 42 % Show Supplier Material materials with Nickel of 42 % |
Technological properties
Property | ||
---|---|---|
Application areas | Invar 42 is used mainly in: |