Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 2.8 - 2.9 g/cm³ Show Supplier Material materials with Dichte of 2.8 - 2.9 g/cm³ | |
Binder | AlBO₃ |
Mechanisch
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.8E-6 - 2.9E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.8E-6 - 2.9E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 85 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 85 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 1.00E+15 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1.00E+15 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Thermal Management: very useful as a heat sink in high power electronic applications and electronic packaging materials. High Temperature Environments: equipment for plasma arc welding, diffusion source wafers, and semiconductor crystal growth equipment & processing. Molten Metal Handling: ideal for interface materials used in various molten metal processes. | |
Processing methods | Hot Pressed Sintering, Chemical Vapor Deposition |