Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.6 g/cm³ Show Supplier Material materials with Dichte of 1.6 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 83 MPa Show Supplier Material materials with Biegefestigkeit of 83 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 3.2 GPa Show Supplier Material materials with Biegemodul of 3.2 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 65 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 65 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 44 MPa Show Supplier Material materials with Zugfestigkeit of 44 MPa | ASTM D638 |
Thermisch
Elektrisch
Technological properties
Property | ||
---|---|---|
Fillers | 20% Glass Bead |