Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.49 g/cm³ Show Supplier Material materials with Dichte of 1.49 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 200 MPa Show Supplier Material materials with Biegefestigkeit of 200 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 8 GPa Show Supplier Material materials with Biegemodul of 8 GPa | ASTM D790 |
Impact strength, Charpy notched, ASTM | 23.0 °C | 75 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 75 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 125 MPa Show Supplier Material materials with Zugfestigkeit of 125 MPa | ASTM D638 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 245 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 245 °C | ASTM D648 | |
Entflammbarkeit | UL94 HB |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Schrumpfung | 23.0 °C | 0.4 - 0.8 % Show Supplier Material materials with Schrumpfung of 0.4 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Wide machinery, instrumentation, auto parts, electronic and electrical, railways, home appliances, communications, textile machinery, sports and leisure products, tubing, fuel tanks and some precision engineering products. | |
Fillers | 30% Glass Fiber and 15% PTFE |