Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.64 g/cm³ Show Supplier Material materials with Dichte of 1.64 g/cm³ | ISO 1183 |
Recycled Content | 18 % Show Supplier Material materials with Recycled Content of 18 % | ||
Wasserabsorption | 23.0 °C | 0.06 % Show Supplier Material materials with Wasserabsorption of 0.06 % | ASTM D570, 23°C/24hr |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 170 MPa Show Supplier Material materials with Biegefestigkeit of 170 MPa | ISO 178, 2 mm/min |
Biegemodul | 23.0 °C | 10.5 GPa Show Supplier Material materials with Biegemodul of 10.5 GPa | ISO 178, 2 mm/min |
Hardness, Rockwell R | 23.0 °C | 113 [-] Show Supplier Material materials with Hardness, Rockwell R of 113 [-] | ASTM D785 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 6.7 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 6.7 kJ/m² | ISO 180 |
Zugfestigkeit | 23.0 °C | 111 MPa Show Supplier Material materials with Zugfestigkeit of 111 MPa | ISO 527, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Aschegehalt | 23.0 °C | 40 % Show Supplier Material materials with Aschegehalt of 40 % | ASTM D5630 | ||
Heat deflection temperature, 1.80 MPa | 224 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 224 °C | ISO 75 | |||
Schmelzpunkt | 249 °C Show Supplier Material materials with Schmelzpunkt of 249 °C | ISO 3146 | |||
Entflammbarkeit | HB for 3.2 mm sample UL94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1kHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 0.01 [-] | ASTM D150 |
Durchschlagfestigkeit | 23.0 °C | 21.9 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 21.9 kV/mm | ASTM D149, 1.6 mm, 500V/s in oil |
Volume resistivity | 23.0 °C | 1.09E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.09E+15 Ω·cm | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.25 - 0.32 % Show Supplier Material materials with Schrumpfung of 0.25 - 0.32 % | ASTM D955 |
Schrumpfung, diagonal | 23.0 °C | 0.53 - 0.79 % Show Supplier Material materials with Schrumpfung, diagonal of 0.53 - 0.79 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical components (e.g. Brackets, motors, connector, Ignition systems) and structural applications | |
Certifications | RoHS,RECH | |
Color | Black | |
Fillers | 40% Glass Fiber and Mineral Powder | |
Processing methods |