Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 27 - 30 % Show Material materials with Dehnung of 27 - 30 % |
Härte, Brinell | 23.0 °C | 70 - 120 [-] Show Material materials with Härte, Brinell of 70 - 120 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 105 MPa Show Material materials with Streckgrenze Rp 0,2 of 105 MPa |
Zugfestigkeit | 23.0 °C | 280 - 310 MPa Show Material materials with Zugfestigkeit of 280 - 310 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Salt water pipes and fittings, hot water tanks, salt water baffles, propeller sleeves, valve and pump components, flanges, boat hulls, marine fittings and marine hardware;Chemical processing: Heat exchanger and cooling plant, evaporator tubes, pump and valve trim;Other: Power steering tube, brake lines, condenser plates, pressure vessels and distiller tubes | |
Corrosion properties | Excellent resistance to erosion and corrosion in seawater. | |
General machinability | Easily machined |