Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 15 % Show Material materials with Dehnung of 15 % | |
Härte, Brinell | 23.0 °C | 248 [-] Show Material materials with Härte, Brinell of 248 [-] | max. |
Streckgrenze | 23.0 °C | 585 MPa Show Material materials with Streckgrenze of 585 MPa | |
Zugfestigkeit | 23.0 °C | 895 MPa Show Material materials with Zugfestigkeit of 895 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Fasteners, and critical pump/valve components;Aerospace: Turbine shafts, aero engine components and high performance fasteners;Power generation: Components for gas turbines, turbine discs, and turbine blades;Other: Springs, screws, bolts, thrust nozzles and transmission parts | |
Corrosion properties | Very high corrosion resistance | |
General machinability | It has good machinability and machines best in the precipitation-hardened condition when it has a machinability rating 45% that of AISI1212 free-cutting grade. |