Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 14.1 % Show Material materials with Dehnung of 14.1 % | Predicted Value, A200 | ||||
15.7 % Show Material materials with Dehnung of 15.7 % | Predicted Value, A80 | |||||
19.0 % Show Material materials with Dehnung of 19.0 % | Predicted Value, A80 Transverse | |||||
20.1 % Show Material materials with Dehnung of 20.1 % | Predicted Value, Transverse | |||||
20.4 % Show Material materials with Dehnung of 20.4 % | Predicted Value, A5 | |||||
24.2 % Show Material materials with Dehnung of 24.2 % | Predicted Value, A50 | |||||
20 °C | 19 % Show Material materials with Dehnung of 19 % | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | ||||
Flächenreduzierung | 40.5 % Show Material materials with Flächenreduzierung of 40.5 % | Predicted Value | ||||
44.0 % Show Material materials with Flächenreduzierung of 44.0 % | Predicted Value, Transverse | |||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||||
Scherfestigkeit | 559.5 MPa Show Material materials with Scherfestigkeit of 559.5 MPa | Predicted Value | ||||
Schubmodule | 80.3 GPa Show Material materials with Schubmodule of 80.3 GPa | Predicted Value | ||||
Streckgrenze | 259.9 MPa Show Material materials with Streckgrenze of 259.9 MPa | Predicted Value, RP1 | ||||
323.3 MPa Show Material materials with Streckgrenze of 323.3 MPa | Predicted Value, RP1 Transverse | |||||
429.1 MPa Show Material materials with Streckgrenze of 429.1 MPa | Predicted Value, Transverse | |||||
475.1 MPa Show Material materials with Streckgrenze of 475.1 MPa | Predicted Value, RP02 Transverse | |||||
516.7 MPa Show Material materials with Streckgrenze of 516.7 MPa | Predicted Value, RP05 | |||||
535.1 MPa Show Material materials with Streckgrenze of 535.1 MPa | Predicted Value, RP002 | |||||
20 °C | 400 MPa Show Material materials with Streckgrenze of 400 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 440 MPa Show Material materials with Streckgrenze of 440 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 460 MPa Show Material materials with Streckgrenze of 460 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
50 °C | 385 MPa Show Material materials with Streckgrenze of 385 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
50 °C | 425 MPa Show Material materials with Streckgrenze of 425 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
50 °C | 445 MPa Show Material materials with Streckgrenze of 445 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
100 °C | 365 MPa Show Material materials with Streckgrenze of 365 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
100 °C | 405 MPa Show Material materials with Streckgrenze of 405 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
100 °C | 425 MPa Show Material materials with Streckgrenze of 425 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
150 °C | 345 MPa Show Material materials with Streckgrenze of 345 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
150 °C | 385 MPa Show Material materials with Streckgrenze of 385 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
150 °C | 405 MPa Show Material materials with Streckgrenze of 405 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
200 °C | 320 MPa Show Material materials with Streckgrenze of 320 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
200 °C | 360 MPa Show Material materials with Streckgrenze of 360 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
200 °C | 380 MPa Show Material materials with Streckgrenze of 380 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
250 °C | 300 MPa Show Material materials with Streckgrenze of 300 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
250 °C | 340 MPa Show Material materials with Streckgrenze of 340 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
250 °C | 360 MPa Show Material materials with Streckgrenze of 360 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
300 °C | 280 MPa Show Material materials with Streckgrenze of 280 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
300 °C | 320 MPa Show Material materials with Streckgrenze of 320 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
300 °C | 340 MPa Show Material materials with Streckgrenze of 340 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | RP02 | |
Zugfestigkeit | 20 °C | 500 - 720 MPa Show Material materials with Zugfestigkeit of 500 - 720 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | |
20 °C | 500 - 670 MPa Show Material materials with Zugfestigkeit of 500 - 670 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 550 - 720 MPa Show Material materials with Zugfestigkeit of 550 - 720 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 550 - 670 MPa Show Material materials with Zugfestigkeit of 550 - 670 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.95 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.95 1/K | Predicted Value |
Spezifische Wärmekapazität | 449.2 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 449.2 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 36.72 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36.72 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Bor | 0.005 % Show Material materials with Bor of 0.005 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
0.5 % Show Material materials with Chrom of 0.5 % | quenched and tempered (+QT) | EN 10028-6 | Flat | |
Kohlenstoff | 0.18 % Show Material materials with Kohlenstoff of 0.18 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Mangan | 1.7 % Show Material materials with Mangan of 1.7 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Nickel | 1 % Show Material materials with Nickel of 1 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
0.015 % Show Material materials with Schwefel of 0.015 % | quenched and tempered (+QT) | EN 10028-6 | Flat | |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Stickstoff | 0.015 % Show Material materials with Stickstoff of 0.015 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Titan | 0.03 % Show Material materials with Titan of 0.03 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Zirkonium | 0.05 % Show Material materials with Zirkonium of 0.05 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |