Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 14 - 15 % Show Material materials with Dehnung of 14 - 15 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 20.0 °C | 55 % Show Material materials with Flächenreduzierung of 55 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 700 - 800 MPa Show Material materials with Streckgrenze of 700 - 800 MPa | |
Zugfestigkeit | 20.0 °C | 800 - 1250 MPa Show Material materials with Zugfestigkeit of 800 - 1250 MPa |
Chemical properties
Property | Value |
---|---|
Bor | 8E-4 - 5E-3 % Show Material materials with Bor of 8E-4 - 5E-3 % |
Chrom | 0.3 - 0.6 % Show Material materials with Chrom of 0.3 - 0.6 % |
Kohlenstoff | 0.24 - 0.3 % Show Material materials with Kohlenstoff of 0.24 - 0.3 % |
Kupfer | 0.4 % Show Material materials with Kupfer of 0.4 % |
Mangan | 1.1 - 1.4 % Show Material materials with Mangan of 1.1 - 1.4 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |