Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 16.9 % Show Material materials with Dehnung of 16.9 % | Predicted Value, A200 | ||||
17.4 % Show Material materials with Dehnung of 17.4 % | Predicted Value, A80 | |||||
19.1 % Show Material materials with Dehnung of 19.1 % | Predicted Value, A80 Transverse | |||||
20.5 % Show Material materials with Dehnung of 20.5 % | Predicted Value, A5 | |||||
20.5 % Show Material materials with Dehnung of 20.5 % | Predicted Value, Transverse | |||||
22.8 % Show Material materials with Dehnung of 22.8 % | Predicted Value, A50 | |||||
20 °C | 19 % Show Material materials with Dehnung of 19 % | thermomechanically rolled | EN 10028-5 | Flat | ||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | ||||
Flächenreduzierung | 40.4 % Show Material materials with Flächenreduzierung of 40.4 % | Predicted Value | ||||
44.4 % Show Material materials with Flächenreduzierung of 44.4 % | Predicted Value, Transverse | |||||
Härte, Brinell | 248 [-] Show Material materials with Härte, Brinell of 248 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||||
Scherfestigkeit | 558.8 MPa Show Material materials with Scherfestigkeit of 558.8 MPa | Predicted Value | ||||
Schubmodule | 79.7 GPa Show Material materials with Schubmodule of 79.7 GPa | Predicted Value | ||||
Streckgrenze | 255.4 MPa Show Material materials with Streckgrenze of 255.4 MPa | Predicted Value, RP1 | ||||
318.5 MPa Show Material materials with Streckgrenze of 318.5 MPa | Predicted Value, RP1 Transverse | |||||
419.3 MPa Show Material materials with Streckgrenze of 419.3 MPa | Predicted Value, RP02 | |||||
428.8 MPa Show Material materials with Streckgrenze of 428.8 MPa | Predicted Value, Transverse | |||||
460 MPa Show Material materials with Streckgrenze of 460 MPa | Predicted Value, RP02 Transverse | |||||
496 MPa Show Material materials with Streckgrenze of 496 MPa | Predicted Value, RP002 | |||||
511.5 MPa Show Material materials with Streckgrenze of 511.5 MPa | Predicted Value, RP05 | |||||
20 °C | 390 MPa Show Material materials with Streckgrenze of 390 MPa | thermomechanically rolled | EN 10028-5 | Flat | ||
20 °C | 400 MPa Show Material materials with Streckgrenze of 400 MPa | thermomechanically rolled | EN 10028-5 | Flat | ||
20 °C | 420 MPa Show Material materials with Streckgrenze of 420 MPa | thermomechanically rolled | EN 10028-5 | Flat | ||
Zugfestigkeit | 20 °C | 500 - 660 MPa Show Material materials with Zugfestigkeit of 500 - 660 MPa | thermomechanically rolled | EN 10028-5 | Flat |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.74 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.74 1/K | Predicted Value |
Spezifische Wärmekapazität | 453.5 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 453.5 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 38.07 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 38.07 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | thermomechanically rolled | EN 10028-5 | Flat |
Kohlenstoff | 0.16 % Show Material materials with Kohlenstoff of 0.16 % | thermomechanically rolled | EN 10028-5 | Flat |
Mangan | 1.7 % Show Material materials with Mangan of 1.7 % | thermomechanically rolled | EN 10028-5 | Flat |
Molybdän | 0.2 % Show Material materials with Molybdän of 0.2 % | thermomechanically rolled | EN 10028-5 | Flat |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % | thermomechanically rolled | EN 10028-5 | Flat |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | thermomechanically rolled | EN 10028-5 | Flat |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % | thermomechanically rolled | EN 10028-5 | Flat |
Schwefel | 0.008 % Show Material materials with Schwefel of 0.008 % | thermomechanically rolled | EN 10028-5 | Flat |
0.015 % Show Material materials with Schwefel of 0.015 % | thermomechanically rolled | EN 10028-5 | Flat | |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | thermomechanically rolled | EN 10028-5 | Flat |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % | thermomechanically rolled | EN 10028-5 | Flat |
Titan | 0.05 % Show Material materials with Titan of 0.05 % | thermomechanically rolled | EN 10028-5 | Flat |
Vanadium | 0.1 % Show Material materials with Vanadium of 0.1 % | thermomechanically rolled | EN 10028-5 | Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |