Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.85 g/cm³ Show Material materials with Dichte of 7.85 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 210 GPa Show Material materials with Elastizitätsmodul of 210 GPa | |
200.0 °C | 188 GPa Show Material materials with Elastizitätsmodul of 188 GPa | ||
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Steel |
Schubmodule | 20.0 °C | 81 GPa Show Material materials with Schubmodule of 81 GPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 1/K | |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Steel | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 42 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 42 W/(m·K) | |
100.0 °C | 39.8 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 39.8 W/(m·K) | ||
200.0 °C | 37.7 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 37.7 W/(m·K) | ||
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1.6E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.6E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Bor | 8E-4 - 5E-3 % Show Material materials with Bor of 8E-4 - 5E-3 % |
Chrom | 0.8 - 1.1 % Show Material materials with Chrom of 0.8 - 1.1 % |
Kohlenstoff | 0.14 - 0.19 % Show Material materials with Kohlenstoff of 0.14 - 0.19 % |
Kupfer | 0.4 % Show Material materials with Kupfer of 0.4 % |
Mangan | 1 - 1.3 % Show Material materials with Mangan of 1 - 1.3 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % |