Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel |
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel |
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel |
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Value | Comment |
---|---|---|
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Chrom | 0.02 % Show Material materials with Chrom of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Kupfer | 0.02 % Show Material materials with Kupfer of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Molybdän | 0.02 % Show Material materials with Molybdän of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Nickel | 0.02 % Show Material materials with Nickel of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Niobium | 0.08 % Show Material materials with Niobium of 0.08 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Silizium | 0.02 % Show Material materials with Silizium of 0.02 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Titan | 0.08 % Show Material materials with Titan of 0.08 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % | SAE J403 | Plate, Strip, Sheet, Welded Tube |