Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 13.0 % Show Material materials with Dehnung of 13.0 % | Predicted Value, A200 | ||||
13.2 % Show Material materials with Dehnung of 13.2 % | Predicted Value, Transverse | |||||
17.0 % Show Material materials with Dehnung of 17.0 % | Predicted Value, A50 | |||||
17.4 % Show Material materials with Dehnung of 17.4 % | Predicted Value, A80 Transverse | |||||
17.9 % Show Material materials with Dehnung of 17.9 % | Predicted Value, A5 | |||||
20 °C | 10 % Show Material materials with Dehnung of 10 % | thermomechanically rolled | EN 10149-2 | Flat | A80 | |
20 °C | 10 % Show Material materials with Dehnung of 10 % | thermomechanically rolled | EN 10149-2 | Flat | ||
20 °C | 12 % Show Material materials with Dehnung of 12 % | thermomechanically rolled | EN 10149-2 | Flat | A80 | |
20 °C | 12 % Show Material materials with Dehnung of 12 % | thermomechanically rolled | EN 10149-2 | Flat | ||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | ||||
Flächenreduzierung | 38.7 % Show Material materials with Flächenreduzierung of 38.7 % | Predicted Value | ||||
44.1 % Show Material materials with Flächenreduzierung of 44.1 % | Predicted Value, Transverse | |||||
Härte, Brinell | 248 [-] Show Material materials with Härte, Brinell of 248 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||||
Scherfestigkeit | 585.9 MPa Show Material materials with Scherfestigkeit of 585.9 MPa | Predicted Value | ||||
Schubmodule | 80.1 GPa Show Material materials with Schubmodule of 80.1 GPa | Predicted Value | ||||
Streckgrenze | 294.8 MPa Show Material materials with Streckgrenze of 294.8 MPa | Predicted Value, RP1 | ||||
328.8 MPa Show Material materials with Streckgrenze of 328.8 MPa | Predicted Value, RP1 Transverse | |||||
506.8 MPa Show Material materials with Streckgrenze of 506.8 MPa | Predicted Value, RP02 Transverse | |||||
547.5 MPa Show Material materials with Streckgrenze of 547.5 MPa | Predicted Value, RP05 | |||||
551.3 MPa Show Material materials with Streckgrenze of 551.3 MPa | Predicted Value, Transverse | |||||
580.4 MPa Show Material materials with Streckgrenze of 580.4 MPa | Predicted Value, RP02 | |||||
739 MPa Show Material materials with Streckgrenze of 739 MPa | Predicted Value, RP002 | |||||
20 °C | 700 MPa Show Material materials with Streckgrenze of 700 MPa | thermomechanically rolled | EN 10149-2 | Flat | ||
Zugfestigkeit | 20 °C | 750 - 950 MPa Show Material materials with Zugfestigkeit of 750 - 950 MPa | thermomechanically rolled | EN 10149-2 | Flat |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.97 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.97 1/K | Predicted Value |
Spezifische Wärmekapazität | 454.1 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 454.1 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 37.65 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 37.65 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.015 % Show Material materials with Aluminium of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Bor | 0.005 % Show Material materials with Bor of 0.005 % | thermomechanically rolled | EN 10149-2 | Flat |
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % | thermomechanically rolled | EN 10149-2 | Flat |
Mangan | 2.1 % Show Material materials with Mangan of 2.1 % | thermomechanically rolled | EN 10149-2 | Flat |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % | thermomechanically rolled | EN 10149-2 | Flat |
Niobium | 0.09 % Show Material materials with Niobium of 0.09 % | thermomechanically rolled | EN 10149-2 | Flat |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | thermomechanically rolled | EN 10149-2 | Flat |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % | thermomechanically rolled | EN 10149-2 | Flat |
Titan | 0.22 % Show Material materials with Titan of 0.22 % | thermomechanically rolled | EN 10149-2 | Flat |
Vanadium | 0.2 % Show Material materials with Vanadium of 0.2 % | thermomechanically rolled | EN 10149-2 | Flat |