Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 17.4 % Show Material materials with Dehnung of 17.4 % | Predicted Value, A200 | ||||
18.5 % Show Material materials with Dehnung of 18.5 % | Predicted Value, A80 | |||||
20.4 % Show Material materials with Dehnung of 20.4 % | Predicted Value, A80 Transverse | |||||
20.8 % Show Material materials with Dehnung of 20.8 % | Predicted Value, A5 | |||||
21.7 % Show Material materials with Dehnung of 21.7 % | Predicted Value, Transverse | |||||
22.9 % Show Material materials with Dehnung of 22.9 % | Predicted Value, A50 | |||||
20 °C | 22 % Show Material materials with Dehnung of 22 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | ||||
Flächenreduzierung | 42.6 % Show Material materials with Flächenreduzierung of 42.6 % | Predicted Value | ||||
44.7 % Show Material materials with Flächenreduzierung of 44.7 % | Predicted Value, Transverse | |||||
Härte, Brinell | 243 [-] Show Material materials with Härte, Brinell of 243 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||||
Scherfestigkeit | 528.8 MPa Show Material materials with Scherfestigkeit of 528.8 MPa | Predicted Value | ||||
Schubmodule | 80.2 GPa Show Material materials with Schubmodule of 80.2 GPa | Predicted Value | ||||
Streckgrenze | 250.5 MPa Show Material materials with Streckgrenze of 250.5 MPa | Predicted Value, RP1 | ||||
318.7 MPa Show Material materials with Streckgrenze of 318.7 MPa | Predicted Value, RP1 Transverse | |||||
362.7 MPa Show Material materials with Streckgrenze of 362.7 MPa | Predicted Value, RP02 | |||||
391 MPa Show Material materials with Streckgrenze of 391 MPa | Predicted Value, Transverse | |||||
460.2 MPa Show Material materials with Streckgrenze of 460.2 MPa | Predicted Value, RP05 | |||||
466.2 MPa Show Material materials with Streckgrenze of 466.2 MPa | Predicted Value, RP02 Transverse | |||||
484.5 MPa Show Material materials with Streckgrenze of 484.5 MPa | Predicted Value, RP002 | |||||
20 °C | 320 MPa Show Material materials with Streckgrenze of 320 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 325 MPa Show Material materials with Streckgrenze of 325 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 335 MPa Show Material materials with Streckgrenze of 335 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 345 MPa Show Material materials with Streckgrenze of 345 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 355 MPa Show Material materials with Streckgrenze of 355 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
Zugfestigkeit | 20 °C | 430 - 630 MPa Show Material materials with Zugfestigkeit of 430 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | |
20 °C | 430 - 610 MPa Show Material materials with Zugfestigkeit of 430 - 610 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 430 - 600 MPa Show Material materials with Zugfestigkeit of 430 - 600 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 430 - 590 MPa Show Material materials with Zugfestigkeit of 430 - 590 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 440 - 630 MPa Show Material materials with Zugfestigkeit of 440 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 440 - 610 MPa Show Material materials with Zugfestigkeit of 440 - 610 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 440 - 600 MPa Show Material materials with Zugfestigkeit of 440 - 600 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 440 - 590 MPa Show Material materials with Zugfestigkeit of 440 - 590 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 450 - 610 MPa Show Material materials with Zugfestigkeit of 450 - 610 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 450 - 630 MPa Show Material materials with Zugfestigkeit of 450 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 450 - 600 MPa Show Material materials with Zugfestigkeit of 450 - 600 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 450 - 590 MPa Show Material materials with Zugfestigkeit of 450 - 590 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 630 MPa Show Material materials with Zugfestigkeit of 470 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 610 MPa Show Material materials with Zugfestigkeit of 470 - 610 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 600 MPa Show Material materials with Zugfestigkeit of 470 - 600 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 590 MPa Show Material materials with Zugfestigkeit of 470 - 590 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 11.87 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 11.87 1/K | Predicted Value |
Spezifische Wärmekapazität | 456.7 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456.7 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 38.05 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 38.05 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Kohlenstoff | 0.14 % Show Material materials with Kohlenstoff of 0.14 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Kupfer | 0.55 % Show Material materials with Kupfer of 0.55 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Mangan | 1.6 % Show Material materials with Mangan of 1.6 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
0.2 % Show Material materials with Molybdän of 0.2 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar | |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar |
0.5 % Show Material materials with Nickel of 0.5 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
0.035 % Show Material materials with Phosphor of 0.035 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar | |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
0.03 % Show Material materials with Schwefel of 0.03 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar | |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Stickstoff | 0.015 % Show Material materials with Stickstoff of 0.015 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Titan | 0.05 % Show Material materials with Titan of 0.05 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Vanadium | 0.1 % Show Material materials with Vanadium of 0.1 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |