Kohlenstoffarmer Stahl
EN 10025-2 Grade S355J2 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-2 Grade S355K2 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-3 Grade S355N normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-3 Grade S355NL normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-2 Grade S355J2C normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S355K2C normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S355JR normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade S355J0 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade E335 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10025-2 Grade E360 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Medium Carbon Steel
ISO 683-1 Grade C45E quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10025-5 Grade S355J2W normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-5 Grade S355K2W normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S355M thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10025-4 Grade S355ML thermomechanically rolledGeliefert von:
2 Matmatch-Lieferanten
Unclassified Low Alloy Steel
EN 10225 Grade S355G7 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant