Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 20 °C | 7.85 g/cm³ Show Material materials with Dichte of 7.85 g/cm³ | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 18.6 % Show Material materials with Dehnung of 18.6 % | Predicted Value, Transverse | ||||
20.2 % Show Material materials with Dehnung of 20.2 % | Predicted Value, A200 | |||||
22.3 % Show Material materials with Dehnung of 22.3 % | Predicted Value, A5 | |||||
22.5 % Show Material materials with Dehnung of 22.5 % | Predicted Value, A80 Transverse | |||||
37.2 % Show Material materials with Dehnung of 37.2 % | Predicted Value | |||||
39.4 % Show Material materials with Dehnung of 39.4 % | Predicted Value, A50 | |||||
20 °C | 38 % Show Material materials with Dehnung of 38 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | A80 | |
20 °C | 41 % Show Material materials with Dehnung of 41 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | A80 | |
Elastizitätsmodul | -100 °C | 217 GPa Show Material materials with Elastizitätsmodul of 217 GPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | |
20 °C | 212 GPa Show Material materials with Elastizitätsmodul of 212 GPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
100 °C | 207 GPa Show Material materials with Elastizitätsmodul of 207 GPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
200 °C | 199 GPa Show Material materials with Elastizitätsmodul of 199 GPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
300 °C | 192 GPa Show Material materials with Elastizitätsmodul of 192 GPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
400 °C | 184 GPa Show Material materials with Elastizitätsmodul of 184 GPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
500 °C | 175 GPa Show Material materials with Elastizitätsmodul of 175 GPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
600 °C | 164 GPa Show Material materials with Elastizitätsmodul of 164 GPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
Flächenreduzierung | 42.9 % Show Material materials with Flächenreduzierung of 42.9 % | Predicted Value, Transverse | ||||
47.3 % Show Material materials with Flächenreduzierung of 47.3 % | Predicted Value | |||||
Härte, Brinell | 272 [-] Show Material materials with Härte, Brinell of 272 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 20 °C | 0.284 [-] Show Material materials with Poissonzahl of 0.284 [-] | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | |
Scherfestigkeit | 544.1 MPa Show Material materials with Scherfestigkeit of 544.1 MPa | Predicted Value | ||||
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel | ||||
Streckgrenze | 280.5 MPa Show Material materials with Streckgrenze of 280.5 MPa | Predicted Value, RP1 | ||||
280.5 MPa Show Material materials with Streckgrenze of 280.5 MPa | Predicted Value, Transverse | |||||
317.2 MPa Show Material materials with Streckgrenze of 317.2 MPa | Predicted Value, RP1 Transverse | |||||
318.5 MPa Show Material materials with Streckgrenze of 318.5 MPa | Predicted Value, RP05 | |||||
323.2 MPa Show Material materials with Streckgrenze of 323.2 MPa | Predicted Value, RP02 | |||||
478.6 MPa Show Material materials with Streckgrenze of 478.6 MPa | Predicted Value, RP02 Transverse | |||||
494.9 MPa Show Material materials with Streckgrenze of 494.9 MPa | Predicted Value, RP002 | |||||
20 °C | 120 - 180 MPa Show Material materials with Streckgrenze of 120 - 180 MPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
20 °C | 120 - 170 MPa Show Material materials with Streckgrenze of 120 - 170 MPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
Zugfestigkeit | 20 °C | 270 - 350 MPa Show Material materials with Zugfestigkeit of 270 - 350 MPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | |
20 °C | 270 - 330 MPa Show Material materials with Zugfestigkeit of 270 - 330 MPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | -100 °C | 1.08e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.08e-05 1/K | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | |
20 °C | 1.19e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.19e-05 1/K | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
100 °C | 1.25e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.25e-05 1/K | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
200 °C | 1.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3e-05 1/K | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
300 °C | 1.36e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.36e-05 1/K | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
400 °C | 1.41e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.41e-05 1/K | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
500 °C | 1.45e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.45e-05 1/K | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
600 °C | 1.49e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.49e-05 1/K | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
Max. Betriebstemperatur | 383.1 °C Show Material materials with Max. Betriebstemperatur of 383.1 °C | Predicted Value, Long | ||||
500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |||||
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel | ||||
Spezifische Wärmekapazität | -100 °C | 423 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 423 J/(kg·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | |
20 °C | 461 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 461 J/(kg·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
100 °C | 479 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 479 J/(kg·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
200 °C | 499 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 499 J/(kg·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
300 °C | 517 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 517 J/(kg·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
400 °C | 536 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 536 J/(kg·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
500 °C | 558 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 558 J/(kg·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
600 °C | 587 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 587 J/(kg·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
Temperaturleitfähigkeit | 20 °C | 15.9 mm²/s Show Material materials with Temperaturleitfähigkeit of 15.9 mm²/s | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | |
100 °C | 14.3 mm²/s Show Material materials with Temperaturleitfähigkeit of 14.3 mm²/s | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
200 °C | 12.5 mm²/s Show Material materials with Temperaturleitfähigkeit of 12.5 mm²/s | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
300 °C | 10.8 mm²/s Show Material materials with Temperaturleitfähigkeit of 10.8 mm²/s | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
400 °C | 9.2 mm²/s Show Material materials with Temperaturleitfähigkeit of 9.2 mm²/s | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
500 °C | 7.6 mm²/s Show Material materials with Temperaturleitfähigkeit of 7.6 mm²/s | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
600 °C | 6.1 mm²/s Show Material materials with Temperaturleitfähigkeit of 6.1 mm²/s | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
Wärmeleitfähigkeit | 20 °C | 57.5 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 57.5 W/(m·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | |
100 °C | 55.7 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 55.7 W/(m·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
200 °C | 51.9 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 51.9 W/(m·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
300 °C | 47.6 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 47.6 W/(m·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
400 °C | 43.4 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 43.4 W/(m·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
500 °C | 39.6 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 39.6 W/(m·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
600 °C | 36 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 W/(m·K) | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elektrische Leitfähigkeit | 8 S/m Show Material materials with Elektrische Leitfähigkeit of 8 S/m | Predicted Value | ||||
spezifischer Widerstand | 20 °C | 1.1e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.1e-07 Ω·m | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | |
100 °C | 2.3e-07 Ω·m Show Material materials with spezifischer Widerstand of 2.3e-07 Ω·m | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
200 °C | 3.04e-07 Ω·m Show Material materials with spezifischer Widerstand of 3.04e-07 Ω·m | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
300 °C | 3.94e-07 Ω·m Show Material materials with spezifischer Widerstand of 3.94e-07 Ω·m | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
400 °C | 5.01e-07 Ω·m Show Material materials with spezifischer Widerstand of 5.01e-07 Ω·m | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
500 °C | 6.25e-07 Ω·m Show Material materials with spezifischer Widerstand of 6.25e-07 Ω·m | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
600 °C | 7.7e-07 Ω·m Show Material materials with spezifischer Widerstand of 7.7e-07 Ω·m | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kohlenstoff | 0.02 % Show Material materials with Kohlenstoff of 0.02 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Mangan | 0.25 % Show Material materials with Mangan of 0.25 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Titan | 0.3 % Show Material materials with Titan of 0.3 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |