Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.65 - 7.7 g/cm³ Show Material materials with Dichte of 7.65 - 7.7 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 12 - 14 % Show Material materials with Dehnung of 12 - 14 % | |
Dehnung, transversal | 20.0 °C | 5 % Show Material materials with Dehnung, transversal of 5 % | |
Elastizitätsmodul | 20.0 °C | 196 - 216 GPa Show Material materials with Elastizitätsmodul of 196 - 216 GPa | |
100.0 °C | 213 GPa Show Material materials with Elastizitätsmodul of 213 GPa | ||
200.0 °C | 207 GPa Show Material materials with Elastizitätsmodul of 207 GPa | ||
300.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa | ||
400.0 °C | 192 GPa Show Material materials with Elastizitätsmodul of 192 GPa | ||
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Martensitic Stainless Steel |
Streckgrenze | 20.0 °C | 550 MPa Show Material materials with Streckgrenze of 550 MPa | |
Streckgrenze Rp 0,2 | 20.0 °C | 550 MPa Show Material materials with Streckgrenze Rp 0,2 of 550 MPa | |
50.0 °C | 515 MPa Show Material materials with Streckgrenze Rp 0,2 of 515 MPa | ||
100.0 °C | 495 MPa Show Material materials with Streckgrenze Rp 0,2 of 495 MPa | ||
150.0 °C | 475 MPa Show Material materials with Streckgrenze Rp 0,2 of 475 MPa | ||
200.0 °C | 460 MPa Show Material materials with Streckgrenze Rp 0,2 of 460 MPa | ||
250.0 °C | 450 MPa Show Material materials with Streckgrenze Rp 0,2 of 450 MPa | ||
300.0 °C | 430 MPa Show Material materials with Streckgrenze Rp 0,2 of 430 MPa | ||
350.0 °C | 390 MPa Show Material materials with Streckgrenze Rp 0,2 of 390 MPa | ||
400.0 °C | 345 MPa Show Material materials with Streckgrenze Rp 0,2 of 345 MPa | ||
Streckgrenze Rp 0,2, transversal | 20.0 °C | 550 MPa Show Material materials with Streckgrenze Rp 0,2, transversal of 550 MPa | |
Streckgrenze, transversal | 20.0 °C | 550 MPa Show Material materials with Streckgrenze, transversal of 550 MPa | |
Zugfestigkeit | 20.0 °C | 750 - 950 MPa Show Material materials with Zugfestigkeit of 750 - 950 MPa | |
Zugfestigkeit, transversal | 20.0 °C | 750 - 950 MPa Show Material materials with Zugfestigkeit, transversal of 750 - 950 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | -100.0 °C | 9.2E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.2E-6 1/K | |
20.0 °C | 9.9E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.9E-6 1/K | ||
100.0 °C | 1E-5 - 1.03E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.03E-5 1/K | ||
200.0 °C | 1.05E-5 - 1.08E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.05E-5 - 1.08E-5 1/K | ||
300.0 °C | 1.1E-5 - 1.12E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.12E-5 1/K | ||
400.0 °C | 1.1E-5 - 1.16E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.16E-5 1/K | ||
500.0 °C | 1.1E-5 - 1.19E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.19E-5 1/K | ||
600.0 °C | 1.21E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.21E-5 1/K | ||
700.0 °C | 1.24E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.24E-5 1/K | ||
800.0 °C | 1.29E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.29E-5 1/K | ||
900.0 °C | 1.34E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.34E-5 1/K | ||
1000.0 °C | 1.39E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.39E-5 1/K | ||
Schmelzpunkt | 1370 - 1530 °C Show Material materials with Schmelzpunkt of 1370 - 1530 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 450 - 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 450 - 460 J/(kg·K) | |
100.0 °C | 482 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 482 J/(kg·K) | ||
200.0 °C | 506 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 506 J/(kg·K) | ||
300.0 °C | 525 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 525 J/(kg·K) | ||
400.0 °C | 547 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 547 J/(kg·K) | ||
500.0 °C | 576 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 576 J/(kg·K) | ||
600.0 °C | 616 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 616 J/(kg·K) | ||
Temperaturleitfähigkeit | 20.0 °C | 5.7 mm²/s Show Material materials with Temperaturleitfähigkeit of 5.7 mm²/s | |
Wärmeleitfähigkeit | 20.0 °C | 19.6 - 25 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 19.6 - 25 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 6.17E-7 - 7E-7 Ω·m Show Material materials with spezifischer Widerstand of 6.17E-7 - 7E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 15 - 17 % Show Material materials with Chrom of 15 - 17 % |
Kohlenstoff | 0.12 - 0.22 % Show Material materials with Kohlenstoff of 0.12 - 0.22 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 1.5 - 2.5 % Show Material materials with Nickel of 1.5 - 2.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |