Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 17.6 % Show Material materials with Dehnung of 17.6 % | Predicted Value, A200 | ||||
19.0 % Show Material materials with Dehnung of 19.0 % | Predicted Value, A80 Transverse | |||||
21.1 % Show Material materials with Dehnung of 21.1 % | Predicted Value, A5 | |||||
21.6 % Show Material materials with Dehnung of 21.6 % | Predicted Value, Transverse | |||||
23.8 % Show Material materials with Dehnung of 23.8 % | Predicted Value, A50 | |||||
20 °C | 19 % Show Material materials with Dehnung of 19 % | normalized or normalized formed (+N) | EN 10120 | Flat | A80 | |
20 °C | 24 % Show Material materials with Dehnung of 24 % | normalized or normalized formed (+N) | EN 10120 | Flat | ||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Flächenreduzierung | 41.0 % Show Material materials with Flächenreduzierung of 41.0 % | Predicted Value | ||||
42.8 % Show Material materials with Flächenreduzierung of 42.8 % | Predicted Value, Transverse | |||||
Härte, Brinell | 253 [-] Show Material materials with Härte, Brinell of 253 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel | ||||
Scherfestigkeit | 522.4 MPa Show Material materials with Scherfestigkeit of 522.4 MPa | Predicted Value | ||||
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel | ||||
Streckgrenze | 262.2 MPa Show Material materials with Streckgrenze of 262.2 MPa | Predicted Value, RP1 | ||||
329.1 MPa Show Material materials with Streckgrenze of 329.1 MPa | Predicted Value, RP1 Transverse | |||||
351.9 MPa Show Material materials with Streckgrenze of 351.9 MPa | Predicted Value, Transverse | |||||
411.6 MPa Show Material materials with Streckgrenze of 411.6 MPa | Predicted Value, RP05 | |||||
446.4 MPa Show Material materials with Streckgrenze of 446.4 MPa | Predicted Value, RP002 | |||||
467.2 MPa Show Material materials with Streckgrenze of 467.2 MPa | Predicted Value, RP02 Transverse | |||||
20 °C | 355 MPa Show Material materials with Streckgrenze of 355 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | ||
100 °C | 305 MPa Show Material materials with Streckgrenze of 305 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | RP02 | |
150 °C | 285 MPa Show Material materials with Streckgrenze of 285 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | RP02 | |
200 °C | 255 MPa Show Material materials with Streckgrenze of 255 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | RP02 | |
250 °C | 235 MPa Show Material materials with Streckgrenze of 235 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | RP02 | |
300 °C | 216 MPa Show Material materials with Streckgrenze of 216 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | RP02 | |
Zugfestigkeit | 20 °C | 510 - 620 MPa Show Material materials with Zugfestigkeit of 510 - 620 MPa | normalized or normalized formed (+N) | EN 10120 | Flat |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 297.1 °C Show Material materials with Max. Betriebstemperatur of 297.1 °C | Predicted Value, Long |
500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel |
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 7 S/m Show Material materials with Elektrische Leitfähigkeit of 7 S/m | Predicted Value |
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Mangan | 0.7 % Show Material materials with Mangan of 0.7 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Stickstoff | 0.009 % Show Material materials with Stickstoff of 0.009 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Titan | 0.03 % Show Material materials with Titan of 0.03 % | normalized or normalized formed (+N) | EN 10120 | Flat |