Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 10 - 16 % Show Material materials with Dehnung A5 of 10 - 16 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 40 - 50 % Show Material materials with Flächenreduzierung of 40 - 50 % | |
Härte, Brinell | 23.0 °C | 277 - 375 [-] Show Material materials with Härte, Brinell of 277 - 375 [-] | |
Härte, Rockwell C | 23.0 °C | 28 - 40 [-] Show Material materials with Härte, Rockwell C of 28 - 40 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 725 - 1175 MPa Show Material materials with Streckgrenze Rp 0,2 of 725 - 1175 MPa | |
Zugfestigkeit | 23.0 °C | 930 - 1310 MPa Show Material materials with Zugfestigkeit of 930 - 1310 MPa |