Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Dichte of 7.6 - 7.8 g/cm³ | Typical for Ferritic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 22 % Show Material materials with Dehnung A5 of 22 % | |
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Ferritic Stainless Steel |
Härte, Brinell | 23.0 °C | 162 [-] Show Material materials with Härte, Brinell of 162 [-] | |
Härte, Rockwell B | 23.0 °C | 80 [-] Show Material materials with Härte, Rockwell B of 80 [-] | |
Härte, Vickers | 23.0 °C | 175 [-] Show Material materials with Härte, Vickers of 175 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Ferritic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Ferritic Stainless Steel |
Streckgrenze Rp 0,2 | 23.0 °C | 175 MPa Show Material materials with Streckgrenze Rp 0,2 of 175 MPa | |
Zugfestigkeit | 23.0 °C | 360 MPa Show Material materials with Zugfestigkeit of 360 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9.3E-6 - 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.3E-6 - 1.2E-5 1/K | Typical for Ferritic Stainless Steel |
Schmelzpunkt | 1425 - 1530 °C Show Material materials with Schmelzpunkt of 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 420 - 586 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 420 - 586 J/(kg·K) | Typical for Ferritic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 11 - 22 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 11 - 22 W/(m·K) | Typical for Ferritic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 - 7.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Technological properties
Property | ||
---|---|---|
Processing history | annealed |