Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ | Typical for Nickel Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Steel |
Härte, Rockwell C | 20.0 °C | 38.5 - 52.5 [-] Show Material materials with Härte, Rockwell C of 38.5 - 52.5 [-] | |
Härte, Vickers | 20.0 °C | 370 - 570 [-] Show Material materials with Härte, Vickers of 370 - 570 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Steel |
Schubmodule | 23.0 °C | 76 GPa Show Material materials with Schubmodule of 76 GPa | Typical for Nickel Steel |
Zugfestigkeit | 20.0 °C | 1200 - 1800 MPa Show Material materials with Zugfestigkeit of 1200 - 1800 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1316 - 1595 °C Show Material materials with Schmelzpunkt of 1316 - 1595 °C | Typical for Nickel Steel | |
Spezifische Wärmekapazität | 23.0 °C | 456 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456 J/(kg·K) | Typical for Nickel Steel |
Wärmeleitfähigkeit | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.15 % Show Material materials with Chrom of 0.15 % |
Kohlenstoff | 0.72 - 0.78 % Show Material materials with Kohlenstoff of 0.72 - 0.78 % |
Mangan | 0.3 - 0.5 % Show Material materials with Mangan of 0.3 - 0.5 % |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % |
Nickel | 1.8 - 2.1 % Show Material materials with Nickel of 1.8 - 2.1 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |