Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A80, transversal | 20.0 °C | 34 - 41 % Show Material materials with Dehnung A80, transversal of 34 - 41 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze, transversal | 20.0 °C | 120 - 170 MPa Show Material materials with Streckgrenze, transversal of 120 - 170 MPa | |
Zugfestigkeit, transversal | 20.0 °C | 260 - 350 MPa Show Material materials with Zugfestigkeit, transversal of 260 - 350 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % |
Mangan | 0.6 % Show Material materials with Mangan of 0.6 % |
Phosphor | 0.1 % Show Material materials with Phosphor of 0.1 % |
Schwefel | 0.045 % Show Material materials with Schwefel of 0.045 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Titan | 0.3 % Show Material materials with Titan of 0.3 % |