Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.9 g/cm³ Show Material materials with Dichte of 7.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 17 % Show Material materials with Dehnung of 17 % | |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 670 MPa Show Material materials with Streckgrenze of 670 MPa | |
Zugfestigkeit | 23.0 °C | 1030 MPa Show Material materials with Zugfestigkeit of 1030 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K |
Schmelzpunkt | 1370 °C Show Material materials with Schmelzpunkt of 1370 °C | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 14 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 0.35 % Show Material materials with Aluminium of 0 - 0.35 % |
Bor | 0.001 - 0.01 % Show Material materials with Bor of 0.001 - 0.01 % |
Chrom | 13.5 - 16 % Show Material materials with Chrom of 13.5 - 16 % |
Eisen | 49.1 - 59.5 % Show Material materials with Eisen of 49.1 - 59.5 % |
Kohlenstoff | 0 - 0.08 % Show Material materials with Kohlenstoff of 0 - 0.08 % |
Mangan | 0 - 2 % Show Material materials with Mangan of 0 - 2 % |
Molybdän | 1 - 1.5 % Show Material materials with Molybdän of 1 - 1.5 % |
Nickel | 24 - 27 % Show Material materials with Nickel of 24 - 27 % |
Phosphor | 0 - 0.04 % Show Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.03 % Show Material materials with Schwefel of 0 - 0.03 % |
Silizium | 0 - 1 % Show Material materials with Silizium of 0 - 1 % |
Titan | 1.9 - 2.4 % Show Material materials with Titan of 1.9 - 2.4 % |
Vanadium | 0.1 - 0.5 % Show Material materials with Vanadium of 0.1 - 0.5 % |