Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 23 % Show Material materials with Dehnung of 23 % | |
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 23.0 °C | 480 MPa Show Material materials with Streckgrenze of 480 MPa | |
Zugfestigkeit | 23.0 °C | 790 MPa Show Material materials with Zugfestigkeit of 790 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 480 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 480 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 13 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 20.5 - 23.5 % Show Material materials with Chrom of 20.5 - 23.5 % |
Eisen | 52.1 - 62.1 % Show Material materials with Eisen of 52.1 - 62.1 % |
Kohlenstoff | 0 - 0.06 % Show Material materials with Kohlenstoff of 0 - 0.06 % |
Mangan | 4 - 6 % Show Material materials with Mangan of 4 - 6 % |
Molybdän | 1.5 - 3 % Show Material materials with Molybdän of 1.5 - 3 % |
Nickel | 11.5 - 13.5 % Show Material materials with Nickel of 11.5 - 13.5 % |
Niobium | 0.1 - 0.3 % Show Material materials with Niobium of 0.1 - 0.3 % |
Phosphor | 0 - 0.04 % Show Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.03 % Show Material materials with Schwefel of 0 - 0.03 % |
Silizium | 0 - 0.75 % Show Material materials with Silizium of 0 - 0.75 % |
Stickstoff | 0.2 - 0.4 % Show Material materials with Stickstoff of 0.2 - 0.4 % |
Vanadium | 0.1 - 0.3 % Show Material materials with Vanadium of 0.1 - 0.3 % |