Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Abmessung
Property | Value | Comment |
---|---|---|
Breite | 205 - 2300 mm Show Supplier Material materials with Breite of 205 - 2300 mm | |
Dicke | 800 mm Show Supplier Material materials with Dicke of 800 mm | max. |
Länge | 1000 - 6000 mm Show Supplier Material materials with Länge of 1000 - 6000 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 28.2 % Show Supplier Material materials with Dehnung of 28.2 % | |
Elastizitätsmodul | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Elastizitätsmodul of 200 - 210 GPa | Typical for Steels |
Flächenreduzierung | 23.0 °C | 55.6 % Show Supplier Material materials with Flächenreduzierung of 55.6 % | |
Härte, Brinell | 23.0 °C | 156 [-] Show Supplier Material materials with Härte, Brinell of 156 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Supplier Material materials with Poissonzahl of 0.29 [-] | Typical for Steels |
Streckgrenze | 23.0 °C | 360 MPa Show Supplier Material materials with Streckgrenze of 360 MPa | |
Zugfestigkeit | 23.0 °C | 560 MPa Show Supplier Material materials with Zugfestigkeit of 560 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K |
Spezifische Wärmekapazität | 23.0 °C | 477 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 477 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 42.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 42.7 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 2.2E-7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.2E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 0.8 - 1.1 % Show Supplier Material materials with Chrom of 0.8 - 1.1 % |
Eisen | Balance |
Kohlenstoff | 0.28 - 0.33 % Show Supplier Material materials with Kohlenstoff of 0.28 - 0.33 % |
Kupfer | 0.35 % Show Supplier Material materials with Kupfer of 0.35 % |
Mangan | 0.4 - 0.6 % Show Supplier Material materials with Mangan of 0.4 - 0.6 % |
Molybdän | 0.15 - 0.25 % Show Supplier Material materials with Molybdän of 0.15 - 0.25 % |
Nickel | 0.25 % Show Supplier Material materials with Nickel of 0.25 % |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % |
Schwefel | 0.04 % Show Supplier Material materials with Schwefel of 0.04 % |
Silizium | 0.15 - 0.35 % Show Supplier Material materials with Silizium of 0.15 - 0.35 % |